Customization: | Available |
---|---|
Type: | Welding Wire |
Material: | Low Alloy Steel |
Still deciding? Get samples of US$ 0.2/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Non-alloy steel electrode
SH.J507
Implementation standard :
AWS A5.1E7015
Description :
SH·J507 is a non-alloy steel electrode with alkaline coating, which adopts DC reverse welding. All position welding is possible. The welded metal has good plasticity, toughness and crack resistance.
Use:Welding medium carbon steel and some low alloy steel. Such as 09Mn2Si, 16Mn, 09Mn2V and so on.
Note:
1. Before welding, the electrode must be baked at about 350ºC for one hour, and used with baking.
2. Rust, oil, moisture and other impurities must be removed before welding.
3. When welding, narrow path is appropriate, and short arc operation is required.
Chemical composition of deposited metal :(%)
chemical elements |
C | Mn | Si | S | P | Ni | Cr | Mo | V |
standard values |
≤0.15 | ≤1.60 | ≤0.90 | ≤0.035 | ≤0.035 | ≤0.30 | ≤0.20 | ≤0.30 | ≤0.08 |
instantiate | 0.08 | 1.2 | 0.54 | 0.009 | 0.019 | 0.01 | 0.02 | 0.01 | 0.01 |
test item | Yield strength (MPa) | Tensile strength (MPa) | Elongation(%) | ballistic work (J) |
-30 degree centigrade | ||||
standard values |
≥400 | ≥490 | ≥20 | ≥27 |
instantiate | 435 | 540 | 28 | 145 |
Electrode diameter(mm) | 2.5 | 3.2 | 4.0 | 5.0 |
welding current(A) | 60-90 | 90-120 | 140-180 | 180-230 |
To better ensure the safety of your goods, professional, environmentally friendly, convenient and efficient packaging services will be provided.