Customization: | Available |
---|---|
state: | Solid |
pH: | Alkaline |
Still deciding? Get samples of US$ 0.2/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
sj301G
comply with standards ( Standards)
GB/T 5293 S 49A 2 AB-SU26 AWS A5.17: F7A0-EM12K
Flux /Welding wire | Yield Strength( MPa) | tensile strength( MPa) | elongationA(%) | V notched impact toughness test | grade |
SJ301G/SU26 | 419 | 523 | 30 | 76@-20ºC | GB:S 49A 2 AB-SU26 |
model | SiO2+TiO2 | CaO+MgO | Al2O3+MnO | CaF2 | S | P |
SJ301G | 29.25 | 26.05 | 30.67 | 12.3 | 0.022 | 0.032 |
Before welding, the flux must be at about 300-350 ºC(572-662ºF)Bake at room temperature for 2 hours
Before welding, be sure to remove rust, scale, primer and other impurities on the surface of the base material to obtain excellent welding deposited metal.
In the case of multi-layer welding, the root welding of the groove welding requires a small current and welding speed.
Add new flux regularly to prevent flux defects and poor weld bead surface formation caused by reusing flux
25Kg/Bag, 25 Kg/Barrel, 400 Kg/Ton bag
If you need other packaging, please contact us
To better ensure the safety of your goods, professional, environmentally friendly, convenient and efficient packaging services will be provided.